This is for 22, 1 pound lead ingots produced from clip-on wheel weight alloy. All lead has been melted, fluxed and skimmed of steel clips, zinc, trash and dross. All the hassle of the initial melt and cleaning has been taken care of.
This is good lead. It is the same lead I use when making my projectiles and bullets. Given the "average" composition of Clip-on Lead Wheel Weight Alloy (95.25% lead, 4% antimony, 1/2% tin, 1/4% arsenic), BHN hardness will be somewhere between 8 and 10 when air cooled and somewhere in the neighborhood of 18 to 20 when water dropped. Mix with soft lead or other alloys for different hardness ranges.